FENAPOL UP 6157 TAX 30
Brookfield viscosity at 25°C: 650 – 750 TIX index: 27 – 33 Gel time at 25°C: 27 – 33 Exothermic Peak: 160 – 180 Peak Time: 11am – 3pm Styrene content: 42 – 45 HDT: 70 Tensile elongation: 2 Type: ortho Notes: Pre-accelerated, thixotropic resin Certifications: Certified with Lloyd’s Register View Certification
FENAPOL UP 7759 AY 5
Brookfield viscosity at 25°C: 250 – 350 TIX index: 4 – 6 Gel time at 25°C: 4 – 6 Exothermic Peak: 125 – 145 Time to Peak: 5 – 9 Styrene Content: Styrene Free HDT: 70 Tensile elongation: 2 Type: DCPD Notes: Pre accelerated with amine, diluted in VT and HEMA
FENAPOL UP 8162 S 13
Brookfield viscosity at 25°C: 600 – 700 TIX index: 12 – 14 Gel time at 25°C: 12 – 14 Exothermic Peak: 165 – 185 Peak Time: 8 – 12 Styrene content: 31-33 HDT: 70 Tensile elongation: 2.2 Type: Ortho Notes: For seat production and stabilized under UV light
FENAPOL UP 8162 S 15
Brookfield viscosity at 25°C: 800 – 900 TIX Index: 14 – 17 Gel time at 25°C: 14 – 17 Exothermic Peak: 165 – 185 Peak Time: 8 – 12 Styrene content: 30 – 32 HDT: 70 Tensile elongation: 2.2 Type: Ortho Notes: For seat production and stabilized under UV light
FENAPOL UP 6157 TAX 20
Brookfield viscosity at 25°C: 550 – 650 TIX index: 18 – 22 Gel time at 25°C: 18 – 22 Exothermic Peak: 175 – 195 Peak Time: 10am – 2pm Styrene content: 42 – 45 HDT: 70 Tensile elongation: 2 Type: ortho Notes: Pre-accelerated, thixotropic resin Certifications: Certified with Lloyd’s Register
FENAPOL UP 10169 TAX 15
Brookfield viscosity at 25°C: 800 – 900 TIX index: 13 – 16 Gel time at 25°C: 13 – 16 Exothermic Peak: 120 – 140 Peak Time: 7 – 10 Styrene content: 40 – 42 HDT: 55 Tensile elongation: 3.5 Type: Ortho Notes: Pre-accelerated Tixo with low exothermic peak
FENAPOL UP 10169 TAX 25
Brookfield viscosity at 25°C: 850 – 950 TIX index: 24 – 28 Gel time at 25°C: 24 – 28 Exothermic Peak: 120 – 140 Peak Time: 7 – 10 Styrene content: 40 – 42 HDT: 55 Tensile elongation: 3.5 Type: Ortho Notes: Pre-accelerated Tixo with low exothermic peak
FENAPOL UP 11790 A 25
Brookfield viscosity at 25°C: 140 – 200 TIX Index: 21 – 26 Gel time at 25°C: 21 – 26 Exothermic Peak: 140 – 160 Time to Peak: 4 – 9 Styrene content: 32 – 34 HDT: 77 Tensile elongation: 2 Type: Ortho DCPD Notes: Pre accelerated with low exothermic peak
FENAPOL UP 11790 A 35
Brookfield viscosity at 25°C: 140 – 200 TIX index: 32 – 35 Gel time at 25°C: 32 – 35 Exothermic Peak: 135 – 155 Peak Time: 10am – 2pm Styrene content: 32 – 34 HDT: 77 Tensile elongation: 2 Type: Ortho DCPD Notes: Pre accelerated with low exothermic peak
FENAPOL UP 12157 A 55
Brookfield viscosity at 25°C: 400 – 500 TIX index: 51 – 57 Gel time at 25°C: 51 – 57 Exothermic Peak: 160 – 180 Peak Time: 10am – 3pm Styrene content: 34 – 36 HDT: 70 Tensile elongation: 3 Type: Ortho Notes: Pre accelerated for the production of insulating panels at room temperature